(1) 基于表面等离子体共振成像椭偏技术测量超薄膜层光学常数, Measuring optical constants of ultrathin layers using surface-plasmon-resonance-based imaging ellipsometry, Applied Optics, 2017, 第 11 作者
(2) 基于等离子体共振椭偏技术提升超薄膜层表征精度, High-precision measurement of optical constants of ultra-thin coating using surface plasmon resonance spectroscopic ellipsometry in Otto-Bliokh configuration, Optics Express, 2017, 第 1 作者
(3) 采用高精度分光光度计分析各类光学损耗, Measurement of different types of optical loss using high-precision laser photometer, Measurement Science and Technology, 2017, 第 11 作者
(4) 激光预处理技术对散射缺陷和吸收的抑制作用, Mitigation of scattering defect and absorption of DKDP crystals by laser conditioning, Optics Express, 2015, 第 11 作者
(5) 晶体材料缺陷表征分析, Characterization of inclusions in DKDP crystals, Chinese Optics Letters, 2015, 第 11 作者
(6) 连续过滤技术生长的KDP晶体性能分析, Performance of rapid-grown KDP crystals with continuous filtration, High Power Laser Science and Engineering, 2015, 第 1 作者
(7) 利用化学刻蚀和快速成像法揭示熔石英表面损伤诱导源, Combining wet etching and real-time damage event imaging to reveal the most dangerous laser damage initiator in fused silica, Optics Letters, 2013, 第 1 作者
(8) 化学膜表面损伤诱导源分析, Real-time damage event imaging reveals the absorber inducing laser damage with low density in solgel antireflective coatings, J. Opt. Soc. Am. B, 2013, 第 1 作者
(9) 预处理前后DKDP晶体元件透过率变化揭示吸收特性变化, Transmittance increase after laser conditioning reveals absorption properties variation in DKDP crystals, Optics Express, 2012, 第 1 作者
(10) 晶体损伤形貌的波长依赖性揭示损伤机理, Wavelength Dependence of Laser-Induced Bulk Damage Morphology in KDP Crystal: Determination of the Damage Formation Mechanism, Chinese Physics Letters, 2012, 第 1 作者
(11) 研究损伤形貌解释亚表面缺陷特性, Studies of laser damage morphology reveal subsurface feature in fused silica, Surface and Interface Analysis, 2010, 第 1 作者
(12) KDP和DKDP晶体激光损伤特性, Characteristics of 355 nm Laser Damage in KDP and DKDP Crystals, Chinese Physics Letters, 2009, 第 1 作者
(13) KDP和DKDP晶体激光损伤热过程模型, A Thermal Approach to Model Laser Damage in KDP and DKDP Crystals, Chinese Physics Letters, 2009, 第 1 作者
(14) KDP和DKDP晶体表面和体损伤生长机理研究, Growth Characteristics and Mechanism of Surface and Bulk Damage in KDP and DKDP Crystals, Chinese Physics Letters, 2009, 第 1 作者
(15) 不同切向KDP和DKDP晶体的1-on-1和R-on-1损伤测试分析, One-on-One and R-on-One Tests on KDP and DKDP Crystals with Different Orientations, Chinese Physics Letters, 2009, 第 1 作者
(1)Laser conditioning mechanism revealed by defect and absorption variation in the bulk and at the surface of KDP/DKDP crystals 国际激光损伤会议 2016-09-24
(2)Performance of rapid-grown KDP crystals with continuous filtration 环太激光损伤会议 Guohang Hu, Yueliang Wang, Junxiu Chang, Xiaoyi Xie, Yuanan Zhao, Hongji Qi, and Jianda Shao 2015-05-17